We – Beck u. Kaltheuner – offer a wide range of high-quality refractories “Made in Plettenberg”. Many customers are already convinced of our materials and services. The below shown products and their most important typical values are only a selection of the whole assortment. Please do not hesitate to contact us for further information.

  • Show all
  • Aluminium
  • Foundry
  • Blast Furnace
  • Coking Plants
  • Furnace Systems
  • Steel Plant
  • Cement Production


No products were found for your search. Please try with other search parameters.

BEKABLOCK C 31 H 40

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte/Stahlnadeln
applicationVibrieren
max. service temperature [°C]1400
max. grain size [mm]1
chemical analysis 49,6% Al2O3
45,0% SiO2
0,5% Fe2O3
0,9% TiO2
2,9% CaO
material requirement [kg/dm³]2,44
water addition [l/100kg]10,6 - 11,0
permanent linear change [%]+0.0 (1400 °C)
cold crushing strength [N/mm²]140 (400 °C)/ 107 (1000 °C)/ 133 (1200 °C)/ 116 (1400 °C)

BEKABLOCK M 29 H 40

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsMullit/Stahlnadeln
applicationVibrieren
max. service temperature [°C]1400
max. grain size [mm]1
chemical analysis 58,3% Al2O3
35,8% SiO2
0,9% Fe2O3
1,7% TiO2
2,8% CaO
material requirement [kg/dm³]2,62
water addition [l/100kg]9,7 - 10,1
permanent linear change [%]+0,4 (1400 °C)
cold crushing strength [N/mm²]114 (400 °C)/ 140 (1000 °C)/ 136 (1200 °C)/ 136 (1400 °C)

BEKACHEM 84/6

Aluminium
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Korund
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]6
chemical analysis 84,2% Al2O3
2,1% SiO2
0,8% Fe2O3
2,4% TiO2
0,2% CaO
5,5% P2O5
material requirement [kg/dm³]2,83
water addition [l/100kg]6,3 - 6,7
permanent linear change [%]-0,8 (1200 °C)
cold crushing strength [N/mm²]43 (110 °C)/ 63 (800 °C)/ 69 (1000 °C)/ 87 (1200 °C)

BEKACHEM 84/6

Stahlwerk
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Korund
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]6
chemical analysis 84,2% Al2O3
2,1% SiO2
0,8% Fe2O3
2,4% TiO2
0,2% CaO
5,5% P2O5
material requirement [kg/dm³]2,83
water addition [l/100kg]6,3 - 6,7
permanent linear change [%]-0,8 (1200 °C)
cold crushing strength [N/mm²]43 (110 °C)/ 63 (800 °C)/ 69 (1000 °C)/ 87 (1200 °C)

BEKACHEM 84/6

Giesserei
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Korund
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]6
chemical analysis 84,2% Al2O3
2,1% SiO2
0,8% Fe2O3
2,4% TiO2
0,2% CaO
5,5% P2O5
material requirement [kg/dm³]2,83
water addition [l/100kg]6,3 - 6,7
permanent linear change [%]-0,8 (1200 °C)
cold crushing strength [N/mm²]43 (110 °C)/ 63 (800 °C)/ 69 (1000 °C)/ 87 (1200 °C)

BEKACHEM 84/6

Zementherstellung
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Korund
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]6
chemical analysis 84,2% Al2O3
2,1% SiO2
0,8% Fe2O3
2,4% TiO2
0,2% CaO
5,5% P2O5
material requirement [kg/dm³]2,83
water addition [l/100kg]6,3 - 6,7
permanent linear change [%]-0,8 (1200 °C)
cold crushing strength [N/mm²]43 (110 °C)/ 63 (800 °C)/ 69 (1000 °C)/ 87 (1200 °C)

BEKACHEM 86/10

Aluminium
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Korund
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]10
chemical analysis 86,2% Al2O3
4,3% SiO2
0,8% Fe2O3
2,1% TiO2
0,2% CaO
2,8% P2O5
material requirement [kg/dm³]2,90
water addition [l/100kg]5,1 - 5,5
permanent linear change [%]-1,1 (1300 °C)
cold crushing strength [N/mm²]55 (110 °C)/ 93 (800 °C)/ 90 (1000 °C)/ 123 (1300 °C)

BEKACHEM 86/10

Stahlwerk
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Korund
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]10
chemical analysis 86,2% Al2O3
4,3% SiO2
0,8% Fe2O3
2,1% TiO2
0,2% CaO
2,8% P2O5
material requirement [kg/dm³]2,90
water addition [l/100kg]5,1 - 5,5
permanent linear change [%]-1,1 (1300 °C)
cold crushing strength [N/mm²]55 (110 °C)/ 93 (800 °C)/ 90 (1000 °C)/ 123 (1300 °C)

BEKACHEM 86/10

Giesserei
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Korund
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]10
chemical analysis 86,2% Al2O3
4,3% SiO2
0,8% Fe2O3
2,1% TiO2
0,2% CaO
2,8% P2O5
material requirement [kg/dm³]2,90
water addition [l/100kg]5,1 - 5,5
permanent linear change [%]-1,1 (1300 °C)
cold crushing strength [N/mm²]55 (110 °C)/ 93 (800 °C)/ 90 (1000 °C)/ 123 (1300 °C)

BEKACHEM 86/10

Zementherstellung
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Korund
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]10
chemical analysis 86,2% Al2O3
4,3% SiO2
0,8% Fe2O3
2,1% TiO2
0,2% CaO
2,8% P2O5
material requirement [kg/dm³]2,90
water addition [l/100kg]5,1 - 5,5
permanent linear change [%]-1,1 (1300 °C)
cold crushing strength [N/mm²]55 (110 °C)/ 93 (800 °C)/ 90 (1000 °C)/ 123 (1300 °C)

BEKACHEM 86/3

Hochofen
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsKorund
applicationInjizieren/Schütten
max. service temperature [°C]1600
max. grain size [mm]3
chemical analysis 85,8% Al2O3
10,1% SiO2
0,2% Fe2O3
1,7% TiO2
0,2% CaO
1,1% P2O5
material requirement [kg/dm³]2,76
water addition [l/100kg]7,1 - 13,0
permanent linear change [%]-1,0 (1600 °C)
cold crushing strength [N/mm²]17 (110 °C)/ 33 (800 °C)/ 65 (1200 °C)/ 86 (1600 °C)

BEKACHEM 86/3

Stahlwerk
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsKorund
applicationInjizieren/Schütten
max. service temperature [°C]1600
max. grain size [mm]3
chemical analysis 85,8% Al2O3
10,1% SiO2
0,2% Fe2O3
1,7% TiO2
0,2% CaO
1,1% P2O5
material requirement [kg/dm³]2,76
water addition [l/100kg]7,1 - 13,0
permanent linear change [%]-1,0 (1600 °C)
cold crushing strength [N/mm²]17 (110 °C)/ 33 (800 °C)/ 65 (1200 °C)/ 86 (1600 °C)

BEKAFIX 1220/10

Kokerei
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1200
max. grain size [mm]10
chemical analysis 25,2% Al2O3
61,0% SiO2
2,5% Fe2O3
1,0% TiO2
5,0% CaO
material requirement [kg/dm³]2,04
water addition [l/100kg]9,3 - 9,7
permanent linear change [%]-0,3 (1200 °C)
cold crushing strength [N/mm²]75 (110°C)/ 55 (1000°C)/ 80 (1200°C)

Bekafix 1220/10

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1200
max. grain size [mm]10
chemical analysis 25,2% Al2O3
61,0% SiO2
2,5% Fe2O3
1,0% TiO2
5,0% CaO
material requirement [kg/dm³]2,04
water addition [l/100kg]9,3 - 9,7
permanent linear change [%]-0,3 (1200 °C)
cold crushing strength [N/mm²]75 (110°C)/ 55 (1000°C)/ 80 (1200°C)

BEKAFIX 1280/10

Kokerei
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1200
max. grain size [mm]10
chemical analysis 36,8% Al2O3
50,7% SiO2
3,9% Fe2O3
1,2% TiO2
4,9% CaO
material requirement [kg/dm³]2,00
water addition [l/100kg]7,5 - 8,3
permanent linear change [%]+0,3 (1200 °C)
cold crushing strength [N/mm²]85 (110°C)/ 55 (800°C)/ 55 (1000°C)/ 55 (1200 °C)

Bekafix 1280/10

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1200
max. grain size [mm]10
chemical analysis 36,8% Al2O3
50,7% SiO2
3,9% Fe2O3
1,2% TiO2
4,9% CaO
material requirement [kg/dm³]2,00
water addition [l/100kg]7,5 - 8,3
permanent linear change [%]+0,3 (1200 °C)
cold crushing strength [N/mm²]85 (110°C)/ 55 (800°C)/ 55 (1000°C)/ 55 (1200 °C)

BEKAFIX 1300

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1200
max. grain size [mm]6
chemical analysis 47,3% Al2O3
40,5% SiO2
2,3% Fe2O3
material requirement [kg/dm³]1,80
water addition [l/100kg]13
permanent linear change [%]-0,6 (1200 °C)
cold crushing strength [N/mm²]32 (110 °C)/ 18 (1000 °C)/ 19 (1200 °C)

Bekafix 1300

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1200
max. grain size [mm]6
chemical analysis 47,3% Al2O3
40,5% SiO2
2,3% Fe2O3
material requirement [kg/dm³]1,80
water addition [l/100kg]13
permanent linear change [%]-0,6 (1200 °C)
cold crushing strength [N/mm²]32 (110°C)/ 18 (1000°C)/ 19 (1200°C)

BEKAFIX 1500

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte/Bauxit
applicationVibrieren
max. service temperature [°C]1350
max. grain size [mm]6
chemical analysis 55,8% Al2O3
32,5% SiO2
2,0% Fe2O3
material requirement [kg/dm³]2,25
water addition [l/100kg]12
permanent linear change [%]-0,5 (1300 °C)
cold crushing strength [N/mm²]33 (110 °C)/ 19 (1200 °C)/ 21 (1300 °C)

Bekafix 1550

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte/Bauxit
applicationVibrieren
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 56,5% Al2O3
33,0% SiO2
1,9% Fe2O3
1,7% TiO2
4,6% CaO
material requirement [kg/dm³]2,00
water addition [l/100kg]12 - 14
permanent linear change [%]-0,5 (1450 °C)
cold crushing strength [N/mm²]33 (110°C)/ 20 (1200°C)/ 35 (1400°C)/ 38 (1450 °C)

BEKAFIX 1550 B

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 55,3% Al2O3
37,4% SiO2
0,6% Fe2O3
1,1% TiO2
4,6% CaO
material requirement [kg/dm³]2,15
water addition [l/100kg]11,5 - 12,5
permanent linear change [%]+0,1 (1450 °C)
cold crushing strength [N/mm²]60 (110 °C)/ 30 (1000 °C)/ 40 (1400 °C)/ 48 (1450 °C)

Bekafix 1550 B

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 55,3% Al2O3
37,4% SiO2
0,6% Fe2O3
1,1% TiO2
4,6% CaO
material requirement [kg/dm³]2,15
water addition [l/100kg]11,5 - 12,5
permanent linear change [%]+0,1 (1450 °C)
cold crushing strength [N/mm²]60 (110°C)/ 30 (1000°C)/ 40 (1400°C)/ 48 (1450°C)

BEKAFIX 1550 DH

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Schamotte
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]10
chemical analysis 65,1% Al2O3
24,7% SiO2
1,8% Fe2O3
1,9% TiO2
5,2% CaO
material requirement [kg/dm³]2,15
water addition [l/100kg]11,5 - 12,5
permanent linear change [%]+1,2 (1400 °C)
cold crushing strength [N/mm²]69 (110 °C)/ 23 (1200 °C)/ 22 (1300 °C)/ 21 (1400 °C)

BEKAFIX 37 S30 LC

Zementherstellung
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSiC/Schamotte
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]6
chemical analysis 37,1% Al2O3
27,2% SiO2
0,5% Fe2O3
30,3% SiC
material requirement [kg/dm³]2,44
water addition [l/100kg]5,0 - 5,8
permanent linear change [%]-0,65 (1550 °C)
cold crushing strength [N/mm²]130 (110 °C)/ 160 (1000 °C)/ 160 (1550 °C)

BEKAFIX 40

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationAnwerfen/Spritzen
max. service temperature [°C]1300
max. grain size [mm]3
chemical analysis 45,5% Al2O3
40,7% SiO2
3,5% Fe2O3
1,6% TiO2
6,0% CaO
material requirement [kg/dm³]1,89
water addition [l/100kg]12,5 - 13,5
permanent linear change [%]+0,7 (1300 °C)
cold crushing strength [N/mm²]27 (110 °C)/ 25 (1000 °C)/ 22 (1200 °C) 62 (1300 °C)

Bekafix 40

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationAnwerfen/Spritzen
max. service temperature [°C]1300
max. grain size [mm]3
chemical analysis 45,5% Al2O3
40,7% SiO2
3,5% Fe2O3
1,6% TiO2
6,0% CaO
material requirement [kg/dm³]1,89
water addition [l/100kg]12,5 - 13,5
permanent linear change [%]+0,7 (1300 °C)
cold crushing strength [N/mm²]27 (110 °C)/ 25 (1000 °C)/ 22 (1200 °C) 62 (1300 °C)

BEKAFIX 45 U

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationAnwerfen/Spritzen
max. service temperature [°C]1350
max. grain size [mm]6
chemical analysis 49,1% Al2O3
38,5% SiO2
2,0% Fe2O3
1,8% TiO2
5,9% CaO
material requirement [kg/dm³]1,9
water addition [l/100kg]11 - 15
permanent linear change [%]-0,5 (1200 °C)
cold crushing strength [N/mm²]30 (110°C)/ 20 (1200 °C)

BEKAFIX 45 U

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationAnwerfen/Spritzen
max. service temperature [°C]1350
max. grain size [mm]6
chemical analysis 49,1% Al2O3
38,5% SiO2
2,0% Fe2O3
1,8% TiO2
5,9% CaO
material requirement [kg/dm³]1,9
water addition [l/100kg]11 - 15
permanent linear change [%]-0,5 (1200 °C)
cold crushing strength [N/mm²]30 (110°C)/ 20 (1200°C)

BEKAFIX 45 U

Giesserei
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationAnwerfen/Spritzen
max. service temperature [°C]1350
max. grain size [mm]6
chemical analysis 49,1% Al2O3
38,5% SiO2
2,0% Fe2O3
1,8% TiO2
5,9% CaO
material requirement [kg/dm³]1,9
water addition [l/100kg]11 - 15
permanent linear change [%]-0,5 (1200 °C)
cold crushing strength [N/mm²]30 (110 °C)/ 20 (1200 °C)

Bekafix 50

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationAnwerfen/Spritzen
max. service temperature [°C]1350
max. grain size [mm]6
chemical analysis 50,8% Al2O3
36,3% SiO2
2,2% Fe2O3
material requirement [kg/dm³]1,90
water addition [l/100kg]12
permanent linear change [%]-05 (1200 °C)
cold crushing strength [N/mm²]30 (110°C)/ 20 (1200°C)

Bekafix 50 HF

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationSpritzen
max. service temperature [°C]1400
max. grain size [mm]6
chemical analysis 56,4% Al2O3
32,6% SiO2
0,6% Fe2O3
8,2% CaO
material requirement [kg/dm³]2,1
water addition [l/100kg]12 - 14
permanent linear change [%]-0,4 (1200 °C)
cold crushing strength [N/mm²]80 (110°C)/ 60 (1200°C)

BEKAFIX 50 HFW 1

Hochofen
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationSchütten
max. service temperature [°C]1450
max. grain size [mm]1
chemical analysis 59,7% Al2O3
35,5% SiO2
0,6% Fe2O3
0,7% TiO2
2,4% CaO
material requirement [kg/dm³]2,1
water addition [l/100kg]13,5
permanent linear change [%]-0,3 (1000 °C)
cold crushing strength [N/mm²]40 (110 °C)/ 50 (1000 °C)

BEKAFIX 52 LC

Zementherstellung
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 51,0% Al2O3
44,2% SiO2
0,6% Fe2O3
1,2% TiO2
2,1% CaO
material requirement [kg/dm³]2,30
water addition [l/100kg]5,6 - 6,4
permanent linear change [%]-0,3 (1500 °C)
cold crushing strength [N/mm²]90 (110 °C)/ 100 (1000 °C)/ 130 (1500 °C)

Bekafix 52 LC

Ofen- und Anlagenbau
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 51,0% Al2O3
44,2% SiO2
0,6% Fe2O3
1,2% TiO2
2,1% CaO
material requirement [kg/dm³]2,30
water addition [l/100kg]5,6 - 6,4
permanent linear change [%]-0,3 (1500)
cold crushing strength [N/mm²]90 (110°C)/ 100 (1000°C)/ 130 (1500°C)

Bekafix 52 S6 LC

Ofen- und Anlagenbau
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSiC/Tonerdereiche Rohstoffe
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]6
chemical analysis 52,0% Al2O3
38,0% SiO2
0,7% Fe2O3
5,5% SiC
material requirement [kg/dm³]2,45
water addition [l/100kg]5,7 - 6,3
permanent linear change [%]+0,1 (1550 °C)
cold crushing strength [N/mm²]80 (110 °C)/ 80 (1000 °C)/ 85 (1550 °C)

BEKAFIX 55 CO

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationSpritzen
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 59,0% Al2O3
30,3% SiO2
0,5% Fe2O3
0,9% TiO2
8,2% CaO
material requirement [kg/dm³]2,16
water addition [l/100kg]11,5
permanent linear change [%]-0,3 (1200 °C)
cold crushing strength [N/mm²]85 (110 °C)/ 50 (1200 °C)

Bekafix 55 CO

Hochofen
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationSpritzen
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 59,0% Al2O3
30,3% SiO2
0,5% Fe2O3
0,9% TiO2
8,2% CaO
material requirement [kg/dm³]2,16
water addition [l/100kg]11,5
permanent linear change [%]-0,3 (1200 °C)
cold crushing strength [N/mm²]85 (110°C)/ 50 (1200°C)

BEKAFIX 56 LC

Stahlwerk
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsAndalusit
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]6
chemical analysis 55,7% Al2O3
40,2% SiO2
0,7% Fe2O3
0,7% TiO2
2,0% CaO
material requirement [kg/dm³]2,42
water addition [l/100kg]5,6 - 6,4
permanent linear change [%]+1,3 (1600 °C)
cold crushing strength [N/mm²]74 (110 °C)/ 76 (1000 °C)/ 88 (1500 °C)/ 100 (1600 °C)

Bekafix 56 LC

Ofen- und Anlagenbau
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsAndalusit
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]6
chemical analysis 55,7% Al2O3
40,2% SiO2
0,7% Fe2O3
0,7% TiO2
2,0% CaO
material requirement [kg/dm³]2,42
water addition [l/100kg]5,6 - 6,4
permanent linear change [%]+1,3 (1600 °C)
cold crushing strength [N/mm²]74 (110 °C)/ 76 (1000 °C)/ 88 (1500 °C)/ 100 (1600 °C)

BEKAFIX 57 CO Shot

Hochofen
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationShotcreting
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 61,5% Al2O3
32,9% SiO2
0,5% Fe2O3
material requirement [kg/dm³]2,36
water addition [l/100kg]6,5 - 7,0
permanent linear change [%]-0,2 (1400 °C)
cold crushing strength [N/mm²]136 (110 °C)/ 128 (300 °C)/ 116 (1000 °C)/ 135 (1400 °C)

BEKAFIX 57 Shot

Hochofen
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationShotcreting
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 56,8% Al2O3
37,4% SiO2
0,6% Fe2O3
1,0% TiO2
2,9% CaO
material requirement [kg/dm³]2,34
water addition [l/100kg]7,0 - 7,5
permanent linear change [%]-0,1 (1500 °C)
cold crushing strength [N/mm²]95 (110 °C)/ 95 (800 °C)/ 140 (1500 °C)

Bekafix 60

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte/Bauxit
applicationVibrieren
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 68,0% Al2O3
23,1% SiO2
1,1% Fe2O3
2,1% TiO2
4,6% CaO
material requirement [kg/dm³]2,28
water addition [l/100kg]8,5 - 9,5
permanent linear change [%]-0,7 (1400 °C)
cold crushing strength [N/mm²]94 (110°C)/ 38 (1200°C)/ 52 (1300°C)/ 62 (1400°C)

Bekafix 60 LC

Ofen- und Anlagenbau
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1450
max. grain size [mm]10
chemical analysis 62,2% Al2O3
31,2% SiO2
1,0% Fe2O3
material requirement [kg/dm³]2,54
water addition [l/100kg]5,7 - 6,1
permanent linear change [%]+0,4 (1400 °C)
cold crushing strength [N/mm²]130 (110°C)/ 110 (1000°C)/ 115 (1400°C)

Bekafix 60 ULC

Ofen- und Anlagenbau
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1550
max. grain size [mm]6
chemical analysis 63,2% Al2O3
33,2% SiO2
0,5% Fe2O3
1,1% TiO2
0,9% CaO
material requirement [kg/dm³]2,48
water addition [l/100kg]5,8 - 6,2
permanent linear change [%]+0,5 (1500 °C)
cold crushing strength [N/mm²]35 (110°C)/ 80 (1000 °C)/ 105 (1400°C)/ 120 (1500°C)

BEKAFIX 68 S15 NC

Giesserei
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/SiC
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]6
chemical analysis 68,4% Al2O3
11,8% SiO2
1,2% Fe2O3
15,2% SiC
0,2% CaO
material requirement [kg/dm³]2,76
water addition [l/100kg]4,8 bis 5,4
permanent linear change [%]+0,4 (1500 °C)
cold crushing strength [N/mm²]25 (110 °C)/ 146 (1000 °C)/ 165 (1200 °C)/ 147 (1500 °C)

BEKAFIX 68 ULC

Giesserei
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsMullit
applicationVibrieren
max. service temperature [°C]1550
max. grain size [mm]6
chemical analysis 68,1% Al2O3
28,0% SiO2
0,9% Fe2O3
2,0% TiO2
0,6% CaO
material requirement [kg/dm³]2,50
water addition [l/100kg]5,6 - 6,5
permanent linear change [%]-0,1 (1500 °C)
cold crushing strength [N/mm²]25 (110 °C)/ 90 (1000 °C)/ 105 (1400 °C)/ 180 (1500 °C)

Bekafix 70 2

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationSpritzen
max. service temperature [°C]1350
max. grain size [mm]6
chemical analysis 75,0% Al2O3
13,6% SiO2
1,4% Fe2O3
material requirement [kg/dm³]2,27
water addition [l/100kg]12
permanent linear change [%]-0,5 (1200 °C)
cold crushing strength [N/mm²]22 (110 °C)/ 12 (1000 °C)/ 33 (1400 °C)

BEKAFIX 71/3 LC R

Stahlwerk
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]3
chemical analysis 71,9% Al2O3
21,8% SiO2
1,4% Fe2O3
1,8% TiO2
1,8% CaO
material requirement [kg/dm³]2,39
water addition [l/100kg]7,6 - 8,4
permanent linear change [%]-0,7 (1600 °C)
cold crushing strength [N/mm²]40 (110 °C)/ 80 (1000 °C)/ 90 (1400 °C)/ 130 (1600 °C)

BEKAFIX 73/10 S9 ULC

Zementherstellung
classUlta Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSiC/Bauxit
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]10
chemical analysis 75% Al2O3
12% SiO2
1,1% Fe2O3
8,6% SiC
material requirement [kg/dm³]2,84
water addition [l/100kg]5,0 - 5,5
permanent linear change [%]+0,75 (1550 °C)
cold crushing strength [N/mm²]60 (110 °C)/ 130 (1000 °C)/ 105 (1550 °C)

Bekafix 73/6 S9 ULC-P

Ofen- und Anlagenbau
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/SiC
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]6
chemical analysis 75,2% Al2O3
11,3% SiO2
1,0% Fe2O3
8,6% SiC
1,9% TiO2
0,9% CaO
material requirement [kg/dm³]2,74
water addition [l/100kg]6,0 - 6,6
permanent linear change [%]+1,2 (1500 °C)
cold crushing strength [N/mm²]50 (110°C)/ 160 (1000°C)/ 130 (1500°C)

Bekafix 78 LC

Ofen- und Anlagenbau
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1500
max. grain size [mm]10
chemical analysis 77,8% Al2O3
14,5% SiO2
1,4% Fe2O3
2,4% TiO2
2,5% CaO
material requirement [kg/dm³]2,75
water addition [l/100kg]5,0 - 5,5
permanent linear change [%]-0,0 (1300 °C)
cold crushing strength [N/mm²]142 (110°C)/ 121 (1000°C)/ 123 (1300°C)

BEKAFIX 81 LC

Hochofen
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 68,5% Al2O3
23,0% SiO2
1,1% Fe2O3
material requirement [kg/dm³]2,54
water addition [l/100kg]6,7 - 7,1
permanent linear change [%]-0,5 (1400 °C)
cold crushing strength [N/mm²]120 (110 °C)/ 100 (800 °C)/ 75 (1200 °C)/ 90 (1400 °C)

Bekafix 81 LC

Ofen- und Anlagenbau
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 68,5% Al2O3
23,0% SiO2
1,1% Fe2O3
material requirement [kg/dm³]2,54
water addition [l/100kg]6,7 - 7,1
permanent linear change [%]-0,5 (1400 °C)
cold crushing strength [N/mm²]120 (110 °C)/ 100 (800 °C)/ 75 (1200 °C)/ 90 (1400 °C)

BEKAFIX 81 ULC

Zementherstellung
classUlta Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]6
chemical analysis 83,4% Al2O3
11,4% SiO2
1,0% Fe2O3
2,3% TiO2
0,9% CaO
material requirement [kg/dm³]2,85
water addition [l/100kg]5,5 - 5,7
permanent linear change [%]-1,0 (1600 °C)
cold crushing strength [N/mm²]65 (110°C)/ 155 (1000 °C)/ 170 (1500°C)/ 205 (1600°C)

BEKAFIX 81 ULC

Stahlwerk
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]6
chemical analysis 83,4% Al2O3
11,4% SiO2
1,0% Fe2O3
2,3% TiO2
0,9% CaO
material requirement [kg/dm³]2,85
water addition [l/100kg]5,5 - 5,7
permanent linear change [%]-1,0 (1600 °C)
cold crushing strength [N/mm²]65 (110°C)/ 155 (1000 °C)/ 170 (1500°C)/ 205 (1600°C)

Bekafix 81 ULC

Ofen- und Anlagenbau
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]6
chemical analysis 83,4% Al2O3
11,4% SiO2
1,0% Fe2O3
2,3% TiO2
0,9% CaO
material requirement [kg/dm³]2,85
water addition [l/100kg]5,5 - 5,7
permanent linear change [%]-1,0 (1600 °C)
cold crushing strength [N/mm²]65 (110°C)/ 155 (1000 °C)/ 170 (1500°C)/ 205 (1600°C)

Bekafix 82 HF NC

Ofen- und Anlagenbau
classNo Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]6
chemical analysis 82,0% Al2O3
12,3% SiO2
1,3% Fe2O3
2,6% TiO2
0,2% CaO
material requirement [kg/dm³]2,88
water addition [l/100kg]4,8 - 5,4
permanent linear change [%]-0,1 (1500 °C)
cold crushing strength [N/mm²]20 (110°C)/ 175 (1000°C)/ 200 (1500°C)

Bekafix 82 LC

Ofen- und Anlagenbau
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 81,8% Al2O3
9,6% SiO2
1,2% Fe2O3
material requirement [kg/dm³]2,68
water addition [l/100kg]6,8 - 7,2
permanent linear change [%]-0,9 (1400 °C)
cold crushing strength [N/mm²]135 (110 °C)/ 75 (1000 °C)/ 70 (1400 °C)

BEKAFIX 82 LC/N

Stahlwerk
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]6
chemical analysis 82,0% Al2O3
11,3% SiO2
1,4% Fe2O3
2,6% TiO2
1,7% CaO
material requirement [kg/dm³]2,86
water addition [l/100kg]5,0 - 6,0
permanent linear change [%]-0,4 (1450 °C)
cold crushing strength [N/mm²]138 (110 °C)/ 148 (1000 °C)/ 156 (1450 °C)

BEKAFIX 82 ULC

Stahlwerk
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1700
max. grain size [mm]6
chemical analysis 81,0% Al2O3
13,7% SiO2
1,3% Fe2O3
2,3% TiO2
0,8% CaO
material requirement [kg/dm³]2,71
water addition [l/100kg]5,5 - 6,4
permanent linear change [%]-0,3 (1500 °C)
cold crushing strength [N/mm²]26 (110 °C)/ 78 (1000 °C)/ 188 (1400 °C)/ 166 (1500 °C)

BEKAFIX 82 ULC 3

Stahlwerk
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1720
max. grain size [mm]3
chemical analysis 79,6% Al2O3
14,5% SiO2
1,3% Fe2O3
material requirement [kg/dm³]2,65
water addition [l/100kg]6,3 - 6,7
permanent linear change [%]-0,3 (1500 °C)
cold crushing strength [N/mm²]35 (110 °C)/ 57 (1000 °C)/ 138 (1400 °C)/ 141 (1500 °C)

Bekafix 84 HF ULC

Ofen- und Anlagenbau
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1550
max. grain size [mm]10
chemical analysis 82,2% Al2O3
12,2% SiO2
1,3% Fe2O3
2,5% TiO2
1,0% CaO
material requirement [kg/dm³]2,88
water addition [l/100kg]4,2 - 4,8
permanent linear change [%]+0,2 (1450 °C)
cold crushing strength [N/mm²]133 (110 °C)/ 228 (1000 °C)/225 (1350 °C)/ 202 (1450 °C)

Bekafix 85-10 ULC

Ofen- und Anlagenbau
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsKorund
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]10
chemical analysis 85,4% Al2O3
11,1% SiO2
0,3% Fe2O3
1,7% TiO2
0,9% CaO
material requirement [kg/dm³]3,04
water addition [l/100kg]4,3 - 4,9
permanent linear change [%]+0,1 (1600 °C)
cold crushing strength [N/mm²]80 (110°C)/ 120 (1000°C)/ 190 (1400°C)/ 188 (1600°C)

BEKAFIX 86 ULC

Stahlwerk
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde
applicationVibrieren
max. service temperature [°C]1750
max. grain size [mm]6
chemical analysis 83,2% Al2O3
14,8% SiO2
0,3% Fe2O3
0,2% TiO2
0,6% CaO
material requirement [kg/dm³]2,79
water addition [l/100kg]5,0 - 5,8
permanent linear change [%]+0,7 (1650 °C)
cold crushing strength [N/mm²]40 (110 °C)/ 85 (1000 °C)/ 110 (1650 °C)

Bekafix 90 HW

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsTonerdereiche Rohstoffe
applicationSchütten
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 87,0% Al2O3
0,4% SiO2
0,05% Fe2O3
material requirement [kg/dm³]2,20
water addition [l/100kg]13 - 19
permanent linear change [%]-0,7 (1400 °C)
cold crushing strength [N/mm²]30 (110°C)/ 17 (1000°C)/ 30 (1400°C)

BEKAFIX 90 LW

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsTonerdereiche Rohstoffe
applicationSchütten
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 84,3% Al2O3
0,1% SiO2
0,1% Fe2O3
material requirement [kg/dm³]1,0
water addition [l/100kg]55 - 60
permanent linear change [%]-0,9 (1400 °C)
cold crushing strength [N/mm²]7,5 (110 °C)/ 5,5 (1000 °C)/ 6,5 (1200 °C)

BEKAFIX 90 MW

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsTonerdereiche Rohstoffe
applicationSchütten
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 84,9% Al2O3
0,3% SiO2
0,1% Fe2O3
material requirement [kg/dm³]1,68
water addition [l/100kg]25
permanent linear change [%]-1,0 (1400 °C)
cold crushing strength [N/mm²]13 (110 °C)/ 7 (1000 °C)/ 5 (1200 °C)

BEKAFIX 93 MA 5

Stahlwerk
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde/Spinell
applicationVibrieren
max. service temperature [°C]>1700
max. grain size [mm]10
chemical analysis 93,1% Al2O3
0,1% SiO2
0,1% Fe2O3
0,1% TiO2
1,4% CaO
5,0% MgO
material requirement [kg/dm³]2,96
water addition [l/100kg]4,7 - 5,3
permanent linear change [%]-0,2 (1600 °C)
cold crushing strength [N/mm²]60 (110 °C)/ 69 (1000 °C)/ 144 (1600 °C)

BEKAFIX 93/6 MA 5

Stahlwerk
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde/Spinell
applicationVibrieren
max. service temperature [°C]>1700
max. grain size [mm]6
chemical analysis 92,9% Al2O3
0,1% SiO2
0,1% Fe2O3
0,1% TiO2
1,4% CaO
5,3% MgO
material requirement [kg/dm³]3,08
water addition [l/100kg]3,9 - 4,5
permanent linear change [%]-0,3 (1600 °C)
cold crushing strength [N/mm²]115 (110 °C)/ 120 (1000 °C)/ >240 (1400 °C)/ >240 (1600 °C)

Bekafix 94 C

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde
applicationVibrieren
max. service temperature [°C]1700
max. grain size [mm]6
chemical analysis 96,2% Al2O3
<0,1% SiO2
0,1% Fe2O3
0,1% TiO2
3,2% CaO
material requirement [kg/dm³]2,87
water addition [l/100kg]6,0 - 6,4
permanent linear change [%]+0,0% (1600 °C)
cold crushing strength [N/mm²]165 (110°C)/ 117 (1000 °C)/ 126 (1400°C)/ 117 (1600°C)

Bekafix 94 G

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde
applicationSpritzen
max. service temperature [°C]1650
max. grain size [mm]3
chemical analysis 93,7% Al2O3
<0,1% SiO2
0,1% Fe2O3
0,1% TiO2
5,8% CaO
material requirement [kg/dm³]2,55
water addition [l/100kg]10 - 11
permanent linear change [%]-0,6 (1600 °C)
cold crushing strength [N/mm²]83 (110°C)/ 45 (1400 °C)/ 43 (1500 °C)/ 40 (1600°C)

BEKAFIX 94/6 MA 3

Stahlwerk
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde/Spinell
applicationVibrieren
max. service temperature [°C]1700
max. grain size [mm]6
chemical analysis 95,0% Al2O3
0,1% SiO2
0,1% Fe2O3
1,4% CaO
3,4% MgO
material requirement [kg/dm³]3,04
water addition [l/100kg]3,8 - 4,0
permanent linear change [%]+ 0,1 (1500 °C)
cold crushing strength [N/mm²]116 (110 °C)/ 150 (1000 °C)/ 137 (1200 °C)/ 220 (1500 °C)

BEKAFIX 95 D

Hochofen
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde
applicationVibrieren
max. service temperature [°C]1700
max. grain size [mm]6
chemical analysis 96,5% Al2O3
0,1% Fe2O3
material requirement [kg/dm³]2,96
water addition [l/100kg]5,7 - 5,9
permanent linear change [%]+0,2 (1600 °C)
cold crushing strength [N/mm²]115 (110 °C)/ 130 (1500 °C)/ 130 (1600 °C)

BEKAFIX 95 D

Stahlwerk
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde
applicationVibrieren
max. service temperature [°C]1700
max. grain size [mm]6
chemical analysis 96,5% Al2O3
0,1% Fe2O3
material requirement [kg/dm³]2,96
water addition [l/100kg]5,7 - 5,9
permanent linear change [%]+0,2 (1600 °C)
cold crushing strength [N/mm²]115 (110 °C)/ 130 (1500 °C)/ 130 (1600 °C)

Bekafix 98 ULC

Ofen- und Anlagenbau
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde
applicationVibrieren
max. service temperature [°C]1700
max. grain size [mm]6
chemical analysis 98,5% Al2O3
<0,1% SiO2
<0,1% Fe2O3
material requirement [kg/dm³]3,13
water addition [l/100kg]4,5
permanent linear change [%]-0,3 (1600 °C)
cold crushing strength [N/mm²]50 (110°C)/ 120 (1500°C)/ 140 (1600°C)

BEKAFIX 98 ULC 2

Ofen- und Anlagenbau
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde
applicationVibrieren
max. service temperature [°C]4,3 - 4,7
max. grain size [mm]6
chemical analysis 98,9% Al2O3
0,1% Fe2O3
0,1% TiO2
0,6% CaO
material requirement [kg/dm³]3,14
water addition [l/100kg]4,3 - 4,7
permanent linear change [%]-0,6 (1600 °C)
cold crushing strength [N/mm²]35 (110 °C)/ 25 (1000 °C)/ 210 (1600 °C)

Bekafix A

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsAndalusit
applicationVibrieren
max. service temperature [°C]1350
max. grain size [mm]6
chemical analysis 64,9% Al2O3
26,6% SiO2
0,9% Fe2O3
material requirement [kg/dm³]2,33
water addition [l/100kg]10 - 11
permanent linear change [%]+1,8 (1400 °C)
cold crushing strength [N/mm²]50 (110°C)/ 25 (1000°C)/ 20 (1400 °C)

BEKAFIX AL 1,4 G

Aluminium
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationSpritzen
max. service temperature [°C]1100
max. grain size [mm]4
chemical analysis 43,1% Al2O3
41,4% SiO2
2,5% Fe2O3
0,9% TiO2
6,1% CaO
material requirement [kg/dm³]1,46
water addition [l/100kg]22,4 - 23,0
permanent linear change [%]-0,2 (1000 °C)
cold crushing strength [N/mm²]37 (110 °C)/ 30 (400 °C)/ 14 (1000 °C)

Bekafix AL 2/2 – 1,8

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsAndalusit
applicationVibrieren/Schütten/Spritzen
max. service temperature [°C]1300
max. grain size [mm]6
chemical analysis 64,8% Al2O3
26,3% SiO2
0,8% Fe2O3
0,9% TiO2
6,6% CaO
material requirement [kg/dm³]1,82
water addition [l/100kg]13,5 - 15,5
permanent linear change [%]+1,1 (1400 °C)
cold crushing strength [N/mm²]32 (110 °C)/ 8 (1200 °C)/ 7 (1300 °C)/ 8 (1400 °C)

BEKAFIX AL 35 LC

Aluminium
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1100
max. grain size [mm]6
chemical analysis 23,6% Al2O3
57,0% SiO2
0,7% Fe2O3
material requirement [kg/dm³]2,06
water addition [l/100kg]8,6 - 9,0
permanent linear change [%]-0,4 (1000 °C)
cold crushing strength [N/mm²]50 (110 °C)/ 45 (800 °C)/ 40 (1000 °C)

BEKAFIX AL 72/6 G

Aluminium
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationSpritzen
max. service temperature [°C]1300
max. grain size [mm]6
chemical analysis 71,6% Al2O3
4,3% SiO2
1,1% Fe2O3
6,1% CaO
8,0% BaO
material requirement [kg/dm³]2,35
water addition [l/100kg]11 - 12
permanent linear change [%]-0,4 (1200 ° C)
cold crushing strength [N/mm²]65 (110 °C)/ 45 (800 °C)/ 15 (1000 °C)/ 25 (1200 °C)

BEKAFIX AL 75/6a

Aluminium
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsKorund
applicationSpritzen
max. service temperature [°C]1300
max. grain size [mm]6
chemical analysis 72,7% Al2O3
2,8% SiO2
0,5% Fe2O3
8,0% CaO
9,0% BaO
material requirement [kg/dm³]2,44
water addition [l/100kg]10 - 11
permanent linear change [%]-0,2 (1000 °C)
cold crushing strength [N/mm²]63 (110 °C)/ 42 (800 °C)/ 23 (1000 °C)

BEKAFIX AL 75/6b

Aluminium
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsKorund
applicationSpritzen
max. service temperature [°C]1300
max. grain size [mm]6
chemical analysis 80,9% Al2O3
1,4% SiO2
0,1% Fe2O3
6,3% CaO
6,0% BaO
material requirement [kg/dm³]2,54
water addition [l/100kg]10 - 11
permanent linear change [%]-0,0 (1000 °C)
cold crushing strength [N/mm²]62 (110 °C)/ 46 (800 °C)/ 29 (1000 °C)

BEKAFIX AL 76 LC

Aluminium
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit
applicationVibrieren
max. service temperature [°C]1400
max. grain size [mm]6
chemical analysis 75,9% Al2O3
7,8% SiO2
1,2% Fe2O3
2,3% TiO2
2,9% CaO
6,0% BaO
material requirement [kg/dm³]2,85
water addition [l/100kg]5,3 - 5,9
permanent linear change [%]-0,0 (1200 °C)
cold crushing strength [N/mm²]125 (110 °C)/ 137 (800 °C)/ 88 (1000 °C)/ 76 (1200 °C)

BEKAFIX AL 80

Aluminium
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsKorund
applicationVibrieren
max. service temperature [°C]1400
max. grain size [mm]6
chemical analysis 82,2% Al2O3
3,1% SiO2
0,1% Fe2O3
5,0% CaO
6,0% BaO
material requirement [kg/dm³]2,96
water addition [l/100kg]5,4 - 5,8
permanent linear change [%]+2,2 (1400 °C)
cold crushing strength [N/mm²]170 (110 °C)/ 150 (800 °C)/ 120 (1200 °C)/ 70 (1400 °C)

BEKAFIX AL 82 LC

Aluminium
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsKorund
applicationVibrieren
max. service temperature [°C]1400
max. grain size [mm]6
chemical analysis 82,5% Al2O3
3,2% SiO2
0,1% Fe2O3
1,9% TiO2
2,7% CaO
6,0% BaO
material requirement [kg/dm³]3,18
water addition [l/100kg]4,3 - 4,8
permanent linear change [%]-0,0 (1200 °C)
cold crushing strength [N/mm²]120 (110 °C)/ 144 (800 °C)/ 103 (1000 °C)/ 115 (1200 °C)

BEKAFIX AL 90 LC

Aluminium
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde
applicationVibrieren
max. service temperature [°C]1100
max. grain size [mm]6
chemical analysis 84,5% Al2O3
2,5% SiO2
0,1% Fe2O3
material requirement [kg/dm³]2,99
water addition [l/100kg]5,0 - 5,4
permanent linear change [%]-0,1 (1000 °C)
cold crushing strength [N/mm²]150 (110 °C)/ 95 (800 °C)/ 75 (1000 °C)

BEKAFIX AL 92 LC

Aluminium
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSintertonerde
applicationVibrieren
max. service temperature [°C]1400
max. grain size [mm]6
chemical analysis 92,4% Al2O3
0,1% SiO2
0,1% Fe2O3
2,5% CaO
4,7% BaO
material requirement [kg/dm³]3,07
water addition [l/100kg]4,2 - 5,0
permanent linear change [%]+2,6 (1400 °C)
cold crushing strength [N/mm²]160 (110 °C)/ 125 (1000 °C)/ 180 (1200 °C)/ 75 (1400 °C)

BEKAFIX AL R 1

Aluminium
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsKorund
applicationAnwerfen/Schmieren
max. service temperature [°C]1200
max. grain size [mm]3
chemical analysis 80,4% Al2O3
1,8% SiO2
0,2% Fe2O3
material requirement [kg/dm³]2,4
water addition [l/100kg]12 - 16
permanent linear change [%]-0,1 (800 °C)
cold crushing strength [N/mm²]25 (110 °C)/ 12 (800 °C)

BEKAFIX AL R 3

Aluminium
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationAnwerfen/Schmieren
max. service temperature [°C]1400
max. grain size [mm]3
chemical analysis 47,5% Al2O3
39,8% SiO2
0,7% Fe2O3
1,3% TiO2
4,1% CaO
3,1% BaO
material requirement [kg/dm³]2,0
water addition [l/100kg]12 - 16
permanent linear change [%]-0,2 (800 °C)
cold crushing strength [N/mm²]30 (110 °C)/ 24 (800 °C)/ 16 (1200 °C)

BEKAFIX AL R 4

Aluminium
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationAnwerfen/Schmieren
max. service temperature [°C]1400
max. grain size [mm]1
chemical analysis 47,5% Al2O3
39,8% SiO2
0,7% Fe2O3
1,3% TiO2
4,1% CaO
3,1% BaO
material requirement [kg/dm³]1,9
water addition [l/100kg]14 - 18
permanent linear change [%]-0,4 (800 °C)
cold crushing strength [N/mm²]24 (110 °C)/ 19 (800 °C)/ 13 (1200 °C)

BEKAFIX AS G

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsAndalusit/Schamotte
applicationSpritzen
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 54,9% Al2O3
36,0% SiO2
0,8% Fe2O3
0,8% TiO2
6,0% CaO
material requirement [kg/dm³]2,35
water addition [l/100kg]11 - 13
permanent linear change [%]+0,1 (1400 °C)
cold crushing strength [N/mm²]74 (110 °C)/ 63 (800 °C)/ 42 (1200 °C)/ 46 (1400 °C)

BEKAFIX AS G

Stahlwerk
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsAndalusit/Schamotte
applicationSpritzen
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 54,9% Al2O3
36,0% SiO2
0,8% Fe2O3
0,8% TiO2
6,0% CaO
material requirement [kg/dm³]2,35
water addition [l/100kg]11 - 13
permanent linear change [%]+ 0,1 ( 1400 °C)
cold crushing strength [N/mm²]74 (110 °C)/ 63 (800 °C)/ 42 (1200 °C)/ 46 (1400 °C)

Bekafix AS G

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsAndalusit/Schamotte
applicationSpritzen
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 54,9% Al2O3
36,0% SiO2
0,8% Fe2O3
0,8% TiO2
6,0% CaO
material requirement [kg/dm³]2,35
water addition [l/100kg]11 - 13
permanent linear change [%]+0,1 (1400 °C)
cold crushing strength [N/mm²]74 (110 °C)/ 63 (800 °C)/ 42 (1200 °C)/ 46 (1400 °C)

Bekafix AS LC

Ofen- und Anlagenbau
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsAndalusit
applicationVibrieren
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 55,6% Al2O3
39,7% SiO2
0,8% Fe2O3
0,6% TiO2
2,5% CaO
material requirement [kg/dm³]2,41
water addition [l/100kg]5,5 - 6,2
permanent linear change [%]+0,5 (1450 °C)
cold crushing strength [N/mm²]91 (110 °C)/ 73 (1000 °C)/ 85 (1400 °C)/ 110 (1450 °C)

BEKAFIX CKT

Kokerei
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1250
max. grain size [mm]10
chemical analysis 34,3% Al2O3
48,2% SiO2
1,3% Fe2O3
1,2% TiO2
3,4% CaO
10,3% MgO
material requirement [kg/dm³]2,05
water addition [l/100kg]8 - 8,4
permanent linear change [%]-0,1 (1200 °C)
cold crushing strength [N/mm²]110 (110 °C)/ 98 (800 °C)/ 73 (1000 °C)/ 103 (1200 °C)

Bekafix CKT

Ofen- und Anlagenbau
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1250
max. grain size [mm]10
chemical analysis 34,3% Al2O3
48,2% SiO2
1,3% Fe2O3
1,2% TiO2
3,4% CaO
10,3% MgO
material requirement [kg/dm³]2,05
water addition [l/100kg]8 - 8,4
permanent linear change [%]-0,1 (1200 °C)
cold crushing strength [N/mm²]110 (110 °C)/ 98 (800 °C)/ 73 (1000 °C)/ 103 (1200 °C)

BEKAFIX CKT R

Kokerei
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationVibrieren
max. service temperature [°C]1250
max. grain size [mm]10
chemical analysis 39,0% Al2O3
47,9% SiO2
1,1% Fe2O3
0,6% TiO2
3,4% CaO
material requirement [kg/dm³]1,82
water addition [l/100kg]11,6 - 12
permanent linear change [%]-0,2 (1200 °C)
cold crushing strength [N/mm²]42 (110 °C)/ 37 (400 °C)/ 33 (800 °C)/ 51 (1200 °C)

BEKAFIX Gun 45

Giesserei
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsSchamotte
applicationSpritzen
max. service temperature [°C]1350
max. grain size [mm]6
chemical analysis 40,9% Al2O3
40,7% SiO2
3,9% Fe2O3
1,3% TiO2
10,1% CaO
material requirement [kg/dm³]1,80
water addition [l/100kg]15
permanent linear change [%]-0,0 (1300 °C)
cold crushing strength [N/mm²]55 (110 °C)/ 40 (1000 °C)/ 32 (1200 °C)/ 34 (1300 °C)

BEKAFIX GUN 58 S5

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsMullit
applicationSpritzen
max. service temperature [°C]1550
max. grain size [mm]6
chemical analysis 58,1% Al2O3
29,9% SiO2
1,0% Fe2O3
3,9% SiC
4,2% CaO
material requirement [kg/dm³]2,60
water addition [l/100kg]7,8 - 8,2
permanent linear change [%]+0,5 (1400 °C)
cold crushing strength [N/mm²]130 (110 °C)/ 115 (800 °C)/ 85 (1200 °C)/ 75 (1400 °C)

BEKAFIX Gun 60 S5

Zementherstellung
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsMullit
applicationSpritzen
max. service temperature [°C]1550
max. grain size [mm]6
chemical analysis 58% Al2O3
30% SiO2
0,9% Fe2O3
4,9% SiC
material requirement [kg/dm³]2,6
water addition [l/100kg]11
permanent linear change [%]+0,3 (1400 °C)
cold crushing strength [N/mm²]40 (110 °C)/ 35 (1000 °C)/ 50 (1400 °C)

BEKAFIX L 0,5 G

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsVermiculit
applicationSpritzen/Vibrieren/Schütten/Stochern
max. service temperature [°C]950
max. grain size [mm]4
chemical analysis 33,5% Al2O3
35,5% SiO2
8,4% Fe2O3
1,5% TiO2
14,2% CaO
material requirement [kg/dm³]0,79 - 0,80
water addition [l/100kg]48 - 82
permanent linear change [%]-1,3 (1000 °C)
cold crushing strength [N/mm²]1 - 2 (110 °C)/ 1 (800 °C)/ 1 (1000 °C)

BEKAFIX L 0,8

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsVermiculit
applicationSchütten/Stochern
max. service temperature [°C]950
max. grain size [mm]8
chemical analysis 26,5% Al2O3
43,7% SiO2
8,6% Fe2O3
1,2% TiO2
11,6% CaO
material requirement [kg/dm³]0,8
water addition [l/100kg]50
permanent linear change [%]-0,3 (800 °C)
cold crushing strength [N/mm²]1,0 (110 °C)/ 0,8 (800 °C)

BEKAFIX L 1,0

Zementherstellung
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsVermiculit
applicationSchütten/Stochern
max. service temperature [°C]1000
max. grain size [mm]8
chemical analysis 26,6% Al2O3
45,0% SiO2
8,1% Fe2O3
1,2% TiO2
10,7% CaO
material requirement [kg/dm³]1,0
water addition [l/100kg]40
permanent linear change [%]-0,3 (1000 °C)
cold crushing strength [N/mm²]2,5 (110 °C)/ 1,4 (800 °C)/ 1,0 (1000 °C)

BEKAFIX L 1,0

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsVermiculit
applicationSchütten/Stochern
max. service temperature [°C]1000
max. grain size [mm]8
chemical analysis 26,6% Al2O3
45,0% SiO2
8,1% Fe2O3
1,2% TiO2
10,7% CaO
material requirement [kg/dm³]1,0
water addition [l/100kg]40
permanent linear change [%]-0,3 (1000 °C)
cold crushing strength [N/mm²]2,5 (110 °C)/ 1,4 (800 °C)/ 1,0 (1000 °C)

BEKAFIX L 1,0 G

Zementherstellung
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationSpritzen/Vibrieren/Schütten/Stochern
max. service temperature [°C]1000
max. grain size [mm]4
chemical analysis 36,9% Al2O3
38,4% SiO2
7,1% Fe2O3
1,4% TiO2
12,1% CaO
material requirement [kg/dm³]1,0 - 1,1
water addition [l/100kg]35 - 50
permanent linear change [%]-0,5 (1000 °C)
cold crushing strength [N/mm²]3 - 5 (110 °C)/ 2 - 4 (800 °C)/ 1 - 2 (1000 °C)

BEKAFIX L 1,0 G

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationSpritzen/Vibrieren/Schütten/Stochern
max. service temperature [°C]1000
max. grain size [mm]4
chemical analysis 36,9% Al2O3
38,4% SiO2
7,1% Fe2O3
1,4% TiO2
12,1% CaO
material requirement [kg/dm³]1,0 - 1,1
water addition [l/100kg]35 - 50
permanent linear change [%]-0,5 (1000 °C)
cold crushing strength [N/mm²]3 - 5 (110 °C)/ 2 - 4 (800 °C)/ 1 - 2 (1000 °C)

BEKAFIX L 1,2 G

Zementherstellung
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationSpritzen/Vibrieren/Schütten/Stochern
max. service temperature [°C]1250
max. grain size [mm]4
chemical analysis 40,5% Al2O3
40,4% SiO2
2,4% Fe2O3
1,5% TiO2
11,9% CaO
1,8% MgO
material requirement [kg/dm³]1,1-1,3
water addition [l/100kg]37-48
permanent linear change [%]-0,8 - -1,3 (1200 °C)
cold crushing strength [N/mm²]3-6 (110 °C)/ 2-5 (800 °C)/ 2-8 (1000 °C)/ 1-8 (1200 °C)

BEKAFIX L 1,2 G

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationSpritzen/Vibrieren/Schütten/Stochern
max. service temperature [°C]1250
max. grain size [mm]4
chemical analysis 40,5% Al2O3
40,4% SiO2
2,4% Fe2O3
1,5% TiO2
11,9% CaO
1,8% MgO
material requirement []1,1-1,3
water addition [l/100kg]37-48
permanent linear change [%]-0,8 - -1,3 (1200 °C)
cold crushing strength [N/mm²]3-6 (110 °C)/ 2-5 (800 °C)/ 2-8 (1000 °C)/ 1-8 (1200 °C)

BEKAFIX L 1,3 G

Zementherstellung
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationSpritzen
max. service temperature [°C]1300
max. grain size [mm]4
chemical analysis 44,5% Al2O3
42,9% SiO2
2,5% Fe2O3
1,0% TiO2
6,1% CaO
material requirement [kg/dm³]1,5
water addition [l/100kg]22,5 - 23,5
permanent linear change [%]-0,5 (1200 °C)
cold crushing strength [N/mm²]27 (110 °C)/ 15 (800 °C)/ 13 (1000 °C)/ 11 (1200 °C)

BEKAFIX L 1,4

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationSchütten/Stochern
max. service temperature [°C]1250
max. grain size [mm]10
chemical analysis 40,1% Al2O3
43,3% SiO2
5,1% Fe2O3
1,3% TiO2
7,9% CaO
material requirement [kg/dm³]1,57
water addition [l/100kg]20 - 22
permanent linear change [%]-0,1 (1300 °C)
cold crushing strength [N/mm²]13 (110 °C)/ 12 (800 °C)/ 8 (1000 °C)/19 (1300 °C)

BEKAFIX L 1,4 G

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationSpritzen
max. service temperature [°C]1250
max. grain size [mm]4
chemical analysis 38,4% Al2O3
43,6% SiO2
5,4% Fe2O3
1,3% TiO2
7,9% CaO
material requirement [kg/dm³]1,45
water addition [l/100kg]20 - 24
permanent linear change [%]-0,3 (1300 °C)
cold crushing strength [N/mm²]9 (110 °C)/ 2 (1000 °C)/ 11 (1200 °C)/ 13 (1300 °C)

BEKAFIX L 1,4 K

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]10
chemical analysis 48,6% Al2O3
41,8% SiO2
1,1% Fe2O3
1,0% TiO2
6,4% CaO
material requirement [kg/dm³]1,6
water addition [l/100kg]17 - 20
permanent linear change [%]-0,5 (1300 °C)
cold crushing strength [N/mm²]60 (110 °C)/ 25 (1000 °C)/ 23 (1300 °C)

BEKAFIX L 1,4 LC

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsLeichtschamotte
applicationVibrieren
max. service temperature [°C]1300
max. grain size [mm]10
chemical analysis 43,4% Al2O3
47,7% SiO2
1,9% Fe2O3
1,0% TiO2
4,4% CaO
material requirement [kg/dm³]1,68
water addition [l/100kg]11,8 - 12,8
permanent linear change [%]-0,4 (1300 °C)
cold crushing strength [N/mm²]70 (110 °C)/ 40 (1000 °C)/ 46 (1200 °C)/ 52 (1300 °C)

Bekafix LHT 1,4

Ofen- und Anlagenbau
classFeuerleichtbeton
binding systemHydraulisch
basic raw materialsHohlkugelkorund
applicationVibrieren
max. service temperature [°C]1700
max. grain size [mm]3
chemical analysis 93,7% Al2O3
0,9% SiO2
<0,1% Fe2O3
material requirement [kg/dm³]1,4
water addition [l/100kg]15
permanent linear change [%]+0,9 (1600 °C)
cold crushing strength [N/mm²]22 (110°C)/ 14 (1300°C)/ 25 (1600°C)

BEKAFIX RH 80-6 Q

Stahlwerk
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/Korund
applicationSpritzen
max. service temperature [°C]1700
max. grain size [mm]3
chemical analysis 84,6% Al2O3
7,6% SiO2
1,2% Fe2O3
2,2% TiO2
3,2% CaO
material requirement [kg/dm³]2,52
water addition [l/100kg]11
permanent linear change [%]-2,2 (1400 °C)
cold crushing strength [N/mm²]36 (110 °C)/ 26 (800 °C)/ 17 (1200 °C)/ 51 (1400 °C)

BEKAFIX TAC 2

Stahlwerk
classDichter Feuerbeton
binding systemHydraulisch
basic raw materialsAndalusit
applicationGießen/Selbstfließend
max. service temperature [°C]1720
max. grain size [mm]2
chemical analysis 58,0% Al2O3
36,9% SiO2
0,9% Fe2O3
0,2% TiO2
3,0% CaO
material requirement [kg/dm³]2,23
water addition [l/100kg]10,8 - 12,8
permanent linear change [%]+0,2 (1450 °C)
cold crushing strength [N/mm²]41 (110 °C)/ 39 (400 °C)/ 38 (1000 °C)

BEKAFIX VH 9 Shot

Hochofen
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsKorund/SiC
applicationShotcreting
max. service temperature [°C]1650
max. grain size [mm]6
chemical analysis 81,5% Al2O3
4,5% SiO2
0,3% Fe2O3
8,5% SiC
material requirement [kg/dm³]3,01
water addition [l/100kg]5,0 - 5,5
permanent linear change [%]0 (1400 °C)
cold crushing strength [N/mm²]134 (110 °C)/ 135 (300 °C)/ 133 (1000 °C)/ 116 (1400 °C)

BEKASOL CAST T

Stahlwerk
classDichter No-Cement Feuerbeton
binding systemSol-Gel
basic raw materialsTonerdereiche Rohstoffe
applicationVibrieren/Selbstfließend
max. service temperature [°C]1700
max. grain size [mm]6
chemical analysis 65,6% Al2O3
30,4% SiO2
0,8% Fe2O3
<0,2% CaO
material requirement [kg/dm³]2,32
permanent linear change [%]-0,1 (1400 °C)
cold crushing strength [N/mm²]37 (110 °C)/ 63 (800 °C)/ 73 (1000 °C)/ 85 (1400 °C)

BEKASOL Gun 60 S

Zementherstellung
classDichter No-Cement Feuerbeton
binding systemSol Gel
basic raw materialsTonerdereiche Rohstoffe
applicationSpritzen
max. service temperature [°C]1600
max. grain size [mm]6
chemical analysis 55,1% Al2O3
34,3% SiO2
1,1% Fe2O3
5,3% SiC
2,3% TiO2
material requirement [kg/dm³]2,2
permanent linear change [%]-0,6 (1200 °C)
cold crushing strength [N/mm²]25 (110 °C)/ 63 (1000 °C)/ 53 (1200 °C)

BEKATAP L EXP

Hochofen
classStichlochmasse
binding systemChemisch
basic raw materialsBauxit/Korund
max. service temperature [°C]1600
max. grain size [mm]3
chemical analysis 53,9% Al2O3
11,9% SiO2
1,4% Fe2O3
13,5% SiC
1,4% TiO2
17,1% C
material requirement [kg/dm³]2,4
permanent linear change [%]2,8 (1400 °C)
cold crushing strength [N/mm²]8 (400 °C)

BEKATAP M EF

Hochofen
classStichlochmasse
binding systemChemisch
basic raw materialsKorund/Schamotte
max. service temperature [°C]1600
max. grain size [mm]3
chemical analysis 38,6% Al2O3
38,2% SiO2
1,7% Fe2O3
7,4% SiC
1,0% TiO2
11,3% C
material requirement [kg/dm³]2,1
permanent linear change [%]0,4 (1400 °C)
cold crushing strength [N/mm²]6 (400 °C)

BEKATAP M/L ECO

Hochofen
classStichlochmasse
binding systemChemisch
basic raw materialsSchamotte/Korund
max. service temperature [°C]1600
max. grain size [mm]3
chemical analysis 44,1% Al2O3
35,2% SiO2
1,1% Fe2O3
7,1% SiC
1,3% TiO2
9,9% C
material requirement [kg/dm³]2,3
permanent linear change [%]2,2 (1400 °C)
cold crushing strength [N/mm²]13 (400 °C)

BEKATAP XS EXP

Hochofen
classStichlochmasse
binding systemChemisch
basic raw materialsQuarz/Schamotte
max. service temperature [°C]1600
max. grain size [mm]3
chemical analysis 20,1% Al2O3
60,6% SiO2
1,2% Fe2O3
0,7% TiO2
16,1% C
material requirement [kg/dm³]2,0
permanent linear change [%]+2,0 (1400 °C)
cold crushing strength [N/mm²]1 (400 °C)

Korudur G 1 DS

Ofen- und Anlagenbau
classRammmasse
binding systemAnorganisch-Chemisch
basic raw materialsSchamotte/Korund
applicationStampfen
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 61,6% Al2O3
34,3% SiO2
0,7% Fe2O3
1,1% TiO2
0,1% CaO
1,2% P2O5
material requirement [kg/dm³]2,64
permanent linear change [%]-0,0 (1400 °C)
cold crushing strength [N/mm²]17 (110 °C)/ 49 (1000 °C)/ 71 (1400 °C)

KORUDUR G 2 W

Ofen- und Anlagenbau
classRammmasse
binding systemKeramisch
basic raw materialsBauxit
applicationStampfen
max. service temperature [°C]1450
max. grain size [mm]6
chemical analysis 64,3% Al2O3
28,2% SiO2
1,8% Fe2O3
material requirement [kg/dm³]2,4
permanent linear change [%]-0,2 (1400 °C)
cold crushing strength [N/mm²]40 (1300 °C)

Korudur GK 2

Ofen- und Anlagenbau
classPlastische Masse
binding systemAnorganisch-Chemisch
basic raw materialsSchamotte
applicationStampfen
max. service temperature [°C]1450
max. grain size [mm]10
chemical analysis 60,5% Al2O3
32,3% SiO2
0,9% Fe2O3
material requirement [kg/dm³]2,66
permanent linear change [%]+0,5 (1350 °C)
cold crushing strength [N/mm²]30 (1350°C)

Korudur H 0 DS

Ofen- und Anlagenbau
classRammmasse
binding systemAnorganisch-Chemisch
basic raw materialsKorund
applicationStampfen
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 81,9% Al2O3
15,3% SiO2
0,5% Fe2O3
material requirement [kg/dm³]2,9
permanent linear change [%]-0,0 (1400 °C)
cold crushing strength [N/mm²]14 (110 °C)/ 56 (1000 °C)/ 68 (1400 °C)

Korudur H 1 DS

Ofen- und Anlagenbau
classRammmasse
binding systemAnorganisch-Chemisch
basic raw materialsKorund
applicationStampfen
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 73,8% Al2O3
23,1% SiO2
0,5% Fe2O3
0,7% TiO2
0,2% CaO
1,1% P2O5
material requirement [kg/dm³]2,86
permanent linear change [%]+0,2 (1400 °C)
cold crushing strength [N/mm²]15 (110 °C)/ 50 (1000 °C)/ 70 (1400 °C)

Korudur H 90 D

Ofen- und Anlagenbau
classRammmasse
binding systemAnorganisch-Chemisch
basic raw materialsSintertonerde
applicationStampfen
max. service temperature [°C]1700
max. grain size [mm]6
chemical analysis 93,1% Al2O3
4,7% SiO2
0,3% Fe2O3
material requirement [kg/dm³]3,18
permanent linear change [%]-0,5 (1600 °C)
cold crushing strength [N/mm²]25 (110°C)/ 70 (1000°C)/ 125 (1600°C)

Korudur HK 0

Ofen- und Anlagenbau
classRammmasse
binding systemAnorganisch-Chemisch
basic raw materialsKorund
applicationStampfen
max. service temperature [°C]1550
max. grain size [mm]6
chemical analysis 79,5% Al2O3
14,7% SiO2
0,5% Fe2O3
material requirement [kg/dm³]2,95
permanent linear change [%]+0,2 (1600 °C)
cold crushing strength [N/mm²]65 (1300°C)

Korudur HK 1

Ofen- und Anlagenbau
classPlastische Masse
binding systemAnorganisch-Chemisch
basic raw materialsSintertonerde
applicationStampfen
max. service temperature [°C]1500
max. grain size [mm]6
chemical analysis 69,0% Al2O3
24,9% SiO2
0,6% Fe2O3
material requirement [kg/dm³]2,78
permanent linear change [%]+0,3 (1350 °C)
cold crushing strength [N/mm²]45 (1350°C)

KORUDUR HR 38

Hochofen
classRammmasse
binding systemAnorganisch/Organisch-Chemisch
basic raw materialsBauxit/SiC
applicationStampfen
max. service temperature [°C]1650
max. grain size [mm]6
chemical analysis 60,6% Al2O3
7,7% SiO2
10,6% SiC
13,2% C
material requirement [kg/dm³]2,52
permanent linear change [%]-0,2 (1000 °C)
cold crushing strength [N/mm²]6 (200 °C)/ 6 (1000 °C)/ 4 (1400 °C)

KORUDUR HR 38 T

Hochofen
classRammmasse
binding systemAnorganisch/Organisch-Chemisch
basic raw materialsBauxit/SiC
applicationStampfen
max. service temperature [°C]1650
max. grain size [mm]6
chemical analysis 60,6% Al2O3
7,7% SiO2
10,6% SiC
13,2% C
material requirement [kg/dm³]2,48
permanent linear change [%]+1,8 (1000 °C)
cold crushing strength [N/mm²]11 (200 °C)/ 4 (1000 °C)/ 2 (1400 °C)

Korudur M 80 K

Ofen- und Anlagenbau
classMörtel
binding systemHydraulisch
basic raw materialsKorund
applicationAnwerfen/Vermörteln
max. service temperature [°C]1700
max. grain size [mm]1
chemical analysis 84,9% Al2O3
10,8% SiO2
0,5% Fe2O3
0,5% TiO2
0,1% CaO
material requirement [kg/dm³]1,90
water addition [l/100kg]25 - 30

Korudur MG 2

Ofen- und Anlagenbau
classMörtel
binding systemHydraulisch
basic raw materialsBauxit
applicationAnwerfen/Vermörteln
max. service temperature [°C]1500
max. grain size [mm]1
chemical analysis 63,2% Al2O3
26,9% SiO2
1,7% Fe2O3
2,7% TiO2
0,4% CaO
material requirement [kg/dm³]1,70
water addition [l/100kg]25 - 30

Korudur MG S

Ofen- und Anlagenbau
classMörtel
binding systemHydraulisch
basic raw materialsSchamotte
applicationAnwerfen/Vermörteln
max. service temperature [°C]1400
max. grain size [mm]1
chemical analysis 38,6% Al2O3
52,4% SiO2
2,1% Fe2O3
1,6% TiO2
0,4% CaO
material requirement [kg/dm³]1,60
water addition [l/100kg]25 - 30

KORUDUR MZ 90

Ofen- und Anlagenbau
classMörtel
binding systemHydraulisch
basic raw materialsKorund
applicationAnwerfen/Vermörteln
max. service temperature [°C]1550
max. grain size [mm]1
chemical analysis 84,5% Al2O3
9,6% SiO2
0,5% Fe2O3
0,5% TiO2
1,8% CaO
material requirement [kg/dm³]2,2
water addition [l/100kg]22 - 27

KORUDUR VH 7/83

Hochofen
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSiC/Korund
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]10
chemical analysis 85,1% Al2O3
2,1% SiO2
0,2% Fe2O3
8,3% SiC
0,9% C
material requirement [kg/dm³]3,13
water addition [l/100kg]3,6 - 4,0
permanent linear change [%]+0,2 (1400 °C)
cold crushing strength [N/mm²]99 (110 °C)/ 103 (1000 °C)/ 86 (1400 °C)

KORUDUR VH 7/83 ST3

Hochofen
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSiC/Korund
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]10
chemical analysis 84,4% Al2O3
2,1% SiO2
0,2% Fe2O3
8,2% SiC
1,0% C
material requirement [kg/dm³]3,2
water addition [l/100kg]3,6 - 4,0
permanent linear change [%]+0,2 (1400 °C)
cold crushing strength [N/mm²]108 (110°C)/ 94 (1000 °C)/ 90 (1400 °C)

KORUDUR VH 72 HOT K

Hochofen
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsKorund/SiC
applicationSpritzen
max. service temperature [°C]1600
max. grain size [mm]6
chemical analysis 71,6% Al2O3
4,2% SiO2
17,8% SiC
material requirement [kg/dm³]2,65
water addition [l/100kg]8,5
permanent linear change [%]-0,4 (1400 °C)
cold crushing strength [N/mm²]26 (110°C)/ 15 (1000°C)/ 15 (1400 °C)

KORUDUR VH 72 Hot T

Hochofen
classLow Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSiC/Korund
applicationSpritzen
max. service temperature [°C]1600
max. grain size [mm]6
chemical analysis 71,6% Al2O3
4,0% SiO2
0,3% Fe2O3
17,8% SiC
6,6% C
material requirement [kg/dm³]2,66
water addition [l/100kg]8,5
permanent linear change [%]-0,5 (1400 °C)
cold crushing strength [N/mm²]26 (110 °C)/ 18 (1000 °C)/ 22 (1400 °C)

KORUDUR VHP 19/73 K

Hochofen
classUlta Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsKorund/SiC
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]10
chemical analysis 72,7% Al2O3
2,9% SiO2
19,1% SiC
material requirement [kg/dm³]3,0
water addition [l/100kg]4,5
permanent linear change [%]+0,1 (1400 °C)
cold crushing strength [N/mm²]85 (110 °C)/ 85 (1000 °C)/ 45 (1400°C)

KORUDUR VHP 19/73 T

Hochofen
classUlta Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSiC/Korund
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]10
chemical analysis 72,7% Al2O3
2,9% SiO2
0,2% Fe2O3
19,1% SiC
3,4% C
material requirement [kg/dm³]2,95
water addition [l/100kg]4,4 - 4,6
permanent linear change [%]-0,0 (1400 °C)
cold crushing strength [N/mm²]60 (110 °C)/ 70 (1000 °C)/ 80 (1400 °C)

KORUDUR VHP 19/73 T STA3

Hochofen
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSiC/Korund
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]10
chemical analysis 70,5% Al2O3
2,8% SiO2
0,2% Fe2O3
18,6% SiC
1,2% C
material requirement [kg/dm³]2,95
water addition [l/100kg]4,3 - 4,7
permanent linear change [%]+0,0 (1400 °C)
cold crushing strength [N/mm²]63 (110 °C)/ 67 (1000 °C)/ 85 (1400 °C)

KORUDUR VHP 20/70 T

Hochofen
classUlta Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsBauxit/SiC
applicationVibrieren
max. service temperature [°C]1600
max. grain size [mm]10
chemical analysis 69,4% Al2O3
4,8% SiO2
0,9% Fe2O3
20,7% SiC
1,5% TiO2
1,2% C
material requirement [kg/dm³]2,72
water addition [l/100kg]5,0 - 5,4
permanent linear change [%]+0,0 (1400 °C)
cold crushing strength [N/mm²]36 (110 °C)/ 65 (1000 °C)/ 85 (1400 °C)

KORUDUR VHP 23/68 K

Hochofen
classUltra Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsKorund/SiC
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]10
chemical analysis 66,9% Al2O3
3,1% SiO2
0,2% Fe2O3
23,9% SiC
3,1% C
material requirement [kg/dm³]2,93
water addition [l/100kg]4,4 - 4,8
permanent linear change [%]+0,7 (1500 °C)
cold crushing strength [N/mm²]68 (110 °C)/ 68 (1000 °C)/ 59 (1400 °C)/ 44 (1500°C)

KORUDUR VHP 23/68 T

Hochofen
classUlta Low Cement Feuerbeton
binding systemHydraulisch
basic raw materialsSiC/Korund
applicationVibrieren
max. service temperature [°C]1650
max. grain size [mm]10
chemical analysis 66,3% Al2O3
3,1% SiO2
0,3% Fe2O3
23,8% SiC
3,3% C
material requirement [kg/dm³]2,88
water addition [l/100kg]4,4 - 4,8
permanent linear change [%]+1,0 (1500 °C)
cold crushing strength [N/mm²]58 (110°C)/ 68 (1000°C)/ 55 (1400 °C)/ 56 (1500 °C)

KORUSOL 13/82

Hochofen
classDichter No-Cement Feuerbeton
binding systemSol-Gel
basic raw materialsTonerdereiche Rohstoffe
applicationVibrieren/Selbstfließend
max. service temperature [°C]1700
max. grain size [mm]6
chemical analysis 81,2% Al2O3
2,6% SiO2
0,1% Fe2O3
15,0% SiC
0,9% C
<0,2% CaO
material requirement [kg/dm³]2,97
permanent linear change [%]+0,1 (1400 °C)
cold crushing strength [N/mm²]50 (110 °C)/ 125 (800 °C)/ 85 (1000 °C)/ 90 (1400 °C)
Cookie-Einstellungen
Auf dieser Website werden Cookie verwendet. Diese werden für den Betrieb der Website benötigt oder helfen uns dabei, die Website zu verbessern.
Alle Cookies zulassen
Auswahl speichern
Individuelle Einstellungen
Individuelle Einstellungen
Dies ist eine Übersicht aller Cookies, die auf der Website verwendet werden. Sie haben die Möglichkeit, individuelle Cookie-Einstellungen vorzunehmen. Geben Sie einzelnen Cookies oder ganzen Gruppen Ihre Einwilligung. Essentielle Cookies lassen sich nicht deaktivieren.
Speichern
Abbrechen
Essenziell (2)
Essenzielle Cookies werden für die grundlegende Funktionalität der Website benötigt.
Cookies anzeigen